First-order polarization process as an alternative to antiferroelectricity

arXiv:2603.27590 · cond-mat.mtrl-sci · Submitted 2026-03-29 · Read on arXiv

Listen

Radio episode about this paper

Transcript

Introduction to the show: ident: Condensed Matter. The day in condensed matter: materials, phases and the measurements under them.

Kai: I'm Kai.

Mira: And I'm Mira, here with Lev.

Kai: We're looking at the paper: "First-order polarization process as an alternative to antiferroelectricity".

Mira: Here's the gist of the paper. First-order polarization process as an alternative to antiferroelectricity shows that appealing double-hysteresis P-E loops can appear from a field-induced abrupt rotation of polarization in non-polar CaTiO3 films Context and Motivation Antiferroelectrics generate significant interest since their polarization versus electric field (PE) curves show typical double-hysteresis loops appealing for various applications Unfortunately, antiferroelectrics are rare.

Kai: The paper investigates whether a similar mechanism could exist in polar materials, leading to a first-order polarization process capable of generating double hysteresis loops without invoking a conventional antipolar ground state.

Mira: They focus on CaTiO3, which can be turned ferroelectric under tensile strain, to explore this idea.

Kai: Experimental Setup and Strain Effects The study utilizes epitaxial thin films of non-polar CaTiO3 grown on differently oriented NdGaO3 substrates using a combination of theoretical and experimental techniques.

Title and authors: Kai: So we’re looking at this paper today titled "First-order polarization process as an alternative to antiferroelectricity". We've already talked about what that means in general, but let's get into the specifics of who wrote it and what they were trying to achieve.

Mira: The authors are a group from different places, which you can see by looking at their affiliations. They’re bringing together solid state physics and theoretical materials physics to tackle this problem.

Lev: I wonder how much experimental work versus simulation is in this paper, because when I look at real hardware development, the gap between theory and what you can actually build is where things get tricky.

Kai: The authors use a combination of theoretical calculations and actual experimental measurements on thin films grown on different substrates to see how strain affects these polarization states.

Mira: That’s the setup. They’re using epitaxial thin films of non-polar CaTiO3 grown on NdGaO3 substrates in two different orientations: (one hundred ten)o and (one)o <ref:2603.27590#pg3>.

Lev: So the substrate orientation dictates the mechanical constraints, which means they are essentially tuning the energy landscape of the CaTiO3 film to see what kind of polarization switching emerges.

Kai: Right. The paper’s goal is to see if this strain-induced tuning can stabilize different polar states that lead to double hysteresis loops without relying on a conventional antiferroelectric ground state.

The paper's summary: Mira: So the paper explains that by applying tensile epitaxial strain, they can tune the energy and polarization landscapes of the CaTiO3 films to stabilize different oxygen octahedral rotation patterns.

Kai: They found that for CaTiO3 films strained on NdGaO3 (one hundred ten)o, when you apply an electric field along apc, you get a well-defined ferroelectric hysteresis loop <ref:2603.27590#pg3>.

Lev: That’s the key finding—a clear response in one direction—but what happens if you switch to the other orientation?

Mira: On the (one)o substrate, they observed a double hysteresis loop when the electric field is applied along bo <ref:2603.27590#pg1>. That specific behavior is what caught their attention.

Kai: And they suggest that this double hysteresis loop in the (one)o case isn't smooth; it comes from an abrupt reorientation of the polarization between two ferroelectric states that are close in energy and separated by a small barrier <ref:2603.27590#pg1>.

Lev: If we translate that to real hardware, does this mean the switching is fast enough for some kind of memory operation?

Mira: It suggests a deterministic first-order polarization process, which they compare to a first-order magnetization process in magnetic systems.

The paper's improvements: Kai: The authors propose a phenomenological framework for this, using an angular expansion U(theta) that captures the energy profile of the polarization. It includes terms like K1 two theta, K2 four theta, and so on.

Mira: This model is used to fit both the relative depths of those two energy minima and also the barrier separating them between those states.

Lev: From my side, I need to know how big that barrier is, because if it’s too high, you don't get switching at room temperature on real hardware; what are the energy scales we’re talking about?

Kai: They found that applying an external electric field can tilt this landscape until the stability switches between the two minima around one hundred forty kilo volts per centimeter at zero Kelvin <ref:2603.27590#pg1>.

Mira: That confirms that the double hysteresis loop is governed by this abrupt and reversible reorientation of the polarization vector, which is analogous to a first-order magnetization process.

Conclusion: Kai: To wrap up, this paper shows that we can use strain engineering to create materials where you get different switching modes depending on the direction of the field.

Mira: The implication is that this offers a unique platform combining energy storage, non-volatile memory operation, and electrocaloric effects of both signs simultaneously.

Lev: From an error correction perspective, having two stable states separated by a small barrier is actually quite useful because it defines the switching dynamics we need to model for real hardware.

Kai: So this work suggests that strain-engineered ferroelastic and antipolar materials are really promising candidates for exploring these first-order polarization processes.

Mira: It opens up a new playground for discovering behavior beyond conventional antiferroelectrics, especially when you consider the predicted opposite signs of the electrocaloric temperature change depending on field orientation.

Lev: That duality between ferroelectric and antiferroelectric-like responses based on field orientation is a very useful concept to design multifunctional systems.

Kai: So we’re looking at this paper, "First-order polarization process as an alternative to antiferroelectricity", which suggests that strain engineering can tune the system into a regime with double hysteresis loops without needing the standard antipolar ground state.

Louis Bastogne, *, Lukas Korosec, *, Evgenios Stylianidis, *, Daniel G. Porter, Gareth Nisbet, *

Theoretical Materials Physics, Université de Liège Department of Quantum Matter Physics, University of Geneva London Centre for Nanotechnology and Department of Physics and Astronomy University College London Solid State Physics Institute TU Wien Diamond Light Source

cond-mat.mtrl-sci

Submitted: 2026-03-29

Updated: 2026-10-29

Code: https://github.com/DiamondLightSource/i16_msmapper

License: http://creativecommons.org/licenses/by/4.0/

Importance score: 79/100

The gist: First-order polarization process as an alternative to antiferroelectricity shows that appealing double-hysteresis P-E loops can appear from a field-induced abrupt rotation of polarization in…

Key concepts

First-order polarization process
This is a type of switching mechanism where polarization doesn't change smoothly but abruptly jumps between two stable states. It is analogous to a first-order magnetization process in magnets, meaning it involves overcoming an energy barrier to switch between distinct configurations, leading to sharp hysteresis loops.
Epitaxial strain
This is the mechanical stress induced on a thin film material when it is grown on a substrate with different lattice parameters. By choosing specific substrates like NdGaO3 (110)o or (001)o, researchers can precisely control the internal strain of CaTiO3 films, which in turn modifies its energy landscape and stabilizes specific polarization states.
Double hysteresis loops
These are characteristic curves showing two distinct switching behaviors when an electric field is applied. In this context, they arise from the abrupt reorientation of polarization between two closely spaced ferroelectric states separated by a small energy barrier, which is a signature of the first-order switching process.

Terminology

Summary

First-order polarization process as an alternative to antiferroelectricity shows that appealing double-hysteresis P-E loops can appear from a field-induced abrupt rotation of polarization in non-polar CaTiO3 films

Context and Motivation

Antiferroelectrics generate significant interest since their polarization versus electric field (PE) curves show typical double-hysteresis loops appealing for various applications Unfortunately, antiferroelectrics are rare. The paper investigates whether a similar mechanism could exist in polar materials, leading to a first-order polarization process capable of generating double hysteresis loops without invoking a conventional antipolar ground state. p. 1

Where the paper says it

In the case where this field-induced transition is reversible under removal of the magnetic field, it can give rise to double-hysteresis M-H loops. One may wonder whether, by analogy, a similar mechanism could exist in polar materials, leading to a first-order polarization process capable of generating double hysteresis loops without invoking a conventional antipolar ground state.

They focus on CaTiO3, which can be turned ferroelectric under tensile strain, to explore this idea. p. 1
Where the paper says it

To explore this idea, we focus on CaTiO3, the archetypal perovskite oxide, which exhibits a non-polar orthorhombic P bnm ground state involving oxygen octahedra rotations but is sometimes seen as an incipient ferroelectric [23, 24]. Lying close to a ferroelectric instability, it was shown to develop a spontaneous polarization under tensile strain or chemical substitution [25–30].

Experimental Setup and Strain Effects

The study utilizes epitaxial thin films of non-polar CaTiO3 grown on differently oriented NdGaO3 substrates using a combination of theoretical and experimental techniques. The authors examine how tensile epitaxial strain can induce and stabilize different polar states in CaTiO3. p. 1

Where the paper says it

Considering epitaxial CaTiO3 films grown on differently oriented NdGaO3 orthorhombic substrates, we show, through a combination of experimental and theoretical approaches, that epitaxial strain can tune the energy and polarization landscapes, stabilize different oxygen octahedral rotation patterns, and ultimately enable deterministic first-order polarization process with associated appealing double hysteresis loops. RESULTS We first examine how tensile epitaxial strain can induce and stabilize different polar states in CaTiO3.

They deposited high-quality CaTiO3 thin films on (110)o and (001)o-oriented NdGaO3 substrates to investigate the effect of strain on the energy landscape. p. 1
Where the paper says it

This testifies to a complex and tunable energy landscape and provides an appealing opportunity to explore the possibility of achieving a first-order polarization process. Epitaxial mechanical constraints To investigate this phenomenon, we have deposited high-quality CaTiO3 thin films on (110)o and (001)o-oriented NdGaO3 substrates, with high structural quality and atomically flat surfaces (see SI-S2) The NdGaO3 substrate adopts the same orthorhombic P bnm phase as bulk CaTiO3.

The difference in mechanical constraints imposed by the two substrate orientations leads to markedly different behavior for the two orientations of films. p. 2
Where the paper says it

For both orientations, X-ray diffraction (XRD) confirms that the films are fully strained, twin-free, and inherit the substrate octahedral rotation pattern across the interface (see SI-S3). Importantly, although they arise from the same material, the mechanical constraints imposed on the CaTiO3 film by the NdGaO3 substrate are significantly different for the two substrate orientations (see SI, Table S2) and should therefore affect the energy landscape differently.

Key Findings on Polarization Switching

The research reveals that epitaxial strain can tune the energy and polarization landscapes, stabilizing different oxygen octahedral rotation patterns and enabling a deterministic first-order polarization process with associated appealing double hysteresis loops. For CaTiO3 films strained on NdGaO3 (110)o, a well-defined ferroelectric hysteresis loop is obtained when the field is applied along apc, whereas only a linear dielectric response is observed along bpc. p. 3

Where the paper says it

2(a) shows that a well-defined ferroelectric hysteresis loop is obtained at 4. 2 K when the field is applied along ⃗apc, whereas only a linear dielectric response is observed along ⃗bpc.

For CaTiO3 films strained on NdGaO3 (001)o, a double hysteresis loop emerges when the field is applied along bo. p. 3
Where the paper says it

In what follows, in order to avoid any ambiguity between both Pm phases, we refer to them respectively as P21nm and P b21m, according to the direction of the main component of their polarization without changing the generality of the following results. We next examine the electrical and dielectric measurements which reveal a marked anisotropy: while a conventional ferroelectric loop is observed when the field is applied along ⃗ao, a double hysteresis loop emerges when the field is applied along ⃗bo (Fig.

This distinct behavior in CaTiO3/NdGaO3(001)o is reproduced in second-principles simulations, suggesting that the observed double hysteresis loop is associated with a discontinuous reorientation of the polarization between two ferroelectric states of distinct orientations that are close in energy and separated by a small energy barrier. p. 6
Where the paper says it

7 polarization between two ferroelectric states of distinct orientations that are close in energy and separated by a small energy barrier. By analogy with magnetism, we propose to call that a first-order polarization process.

Theoretical Framework and Analogy

The authors propose that this directional duality arises from a first-order polarization process, an analogue of first-order magnetization process in magnetic systems. They describe the polarization energy landscape using a minimal angular expansion U(θ) = U0+K1 sin2 θ+K2 sin4 θ+K3 sin6 θ (1). p. 6

Where the paper says it

To capture the NEB energy profile U along the minimum-energy path (Fig. 3 (a)) in a compact form, we consider that it only depends on the orientation θ – respect to ⃗ao – of the spontaneous polarization of amplitude Ps, assumed to be constant, and we fit U(θ) using a minimal angular expansion: U(θ) = U0+K1 sin2 θ+K2 sin4 θ+K3 sin6 θ (1) This fit (Table S3) perfectly reproduces both the relative depth of the two minima and the barrier separating them (Fig.

This phenomenological framework captures the NEB energy profile and fits both the relative depth of the two minima and the barrier separating them. p. 6
Where the paper says it

To capture the NEB energy profile U along the minimum-energy path (Fig. 3 (a)) in a compact form, we consider that it only depends on the orientation θ – respect to ⃗ao – of the spontaneous polarization of amplitude Ps, assumed to be constant, and we fit U(θ) using a minimal angular expansion: U(θ) = U0+K1 sin2 θ+K2 sin4 θ+K3 sin6 θ (1) This fit (Table S3) perfectly reproduces both the relative depth of the two minima and the barrier separating them (Fig.

The application of an external electric field progressively tilts this landscape, leading to a field-induced interchange of stability between competing minima at E ∼ 140 kV/cm at 0 K, confirming that the double hysteresis loop is governed by an abrupt and reversible reorientation of the polarization vector analogous to a first-order magnetization process. p. 6
Where the paper says it

Within this phenomenological framework, the application of an external electric field progressively tilts the energy landscape, leading to a field-induced interchange of stability between the two competing minima at E ∼ 140 kV/cm at 0 K, in good agreement with the coercive field obtained from second-principles molecular dynamics simulations. This agreement confirms that, at the phenomenological level, the double hysteresis loop is governed by an abrupt and reversible reorientation of the polarization vector that is directly analogous to the magnetization reversal characteristic of a first-order magnetization process.

Implications and Future Directions

The results establish first-order polarization processes as a general framework for designing multifunctional ferroelectrics. The coexistence of distinct switching modes, such as ferroelectric-like and antiferroelectric-like responses depending on the orientation of the applied field, offers a unique platform combining energy storage, non-volatile memory operation, and electrocaloric effects of both signs. p. 8

Where the paper says it

A key outcome is that ferroelectric and antiferroelectric-like functionalities coexist within the same material, under identical structural and thermodynamic conditions, and can be selectively accessed by the orientation of the applied electric field. This duality offers a unique platform combining energy storage, non-volatile memory operation, electrocaloric effects of both signs, and neuromorphic functionalities within a single ferroic system.

The study suggests that strain-engineered ferroelastic and antipolar materials constitute a fertile playground for discovering analogous behavior beyond conventional antiferroelectrics. p. 8
Where the paper says it

This duality offers a unique platform combining energy storage, non-volatile memory operation, electrocaloric effects of both signs, and neuromorphic functionalities within a single ferroic system. More broadly, our results establish first-order polarization processes as a general framework for designing multifunctional ferroelectrics, and suggest that strain-engineered ferroelastic and antipolar materials constitute a fertile playground for discovering analogous behavior beyond conventional antiferroelectrics.

The predicted opposite signs of the electrocaloric temperature change depending on field orientation reinforce the close analogy between first-order magnetization process and first-order polarization process. p. 7
Where the paper says it

Indeed, in magnetic systems, first-order magnetization process is often accompanied by magnetocaloric effects [45, 46] of opposite sign depending of the orientation of the applied field; by analogy, first-order polarization process is expected to couple to similar electrocaloric behaviors. Consistent with this picture, we predict from our second-principles model opposite signs of the electrocaloric temperature change depending on field orientation: ∆T < 0 when the electric field is applied perpendicular to the polarization and is in the same range of efficiency compared to conventional antiferroelectics (∆T /∆E 2 = −3×10-5 K cm2 kV-2) [47, 48].

Online Methods

The methods section details various experimental techniques used, including thin film deposition using a home-built off-axis radio-frequency magnetron sputtering system, laboratory x-ray diffraction measurements performed on a Panalytical X’Pert Pro diffractometer, and electrical measurements such as capacitance–voltage measurements and dynamical hysteresis measurements (DHM). First-principles calculations were conducted using the ABINIT software package with a norm conserving pseudo-potential. p. 9

Where the paper says it

Exposures were taken using the Pilatus3-100K area detector and these were remapped into reciprocal space using the msmapper program, part of the Dawn software package [53, 54]. First-principles The first-principles calculation has been done using the ABINIT software package [55] using the norm conserving [56] pseudo-potential with the Wu-Cohen (WC) parametrization for the exchange correlation potential [57] treating the following orbitals as valences state: Ca 3s, 3p, 4s, 3d, Ti 4s, 4p, 4d, 5s and O 2s, 2p.

Second-principles atomistic simulations employed an effective interatomic potential built with the Multibinit package, utilizing a Hybrid molecular dynamics Monte Carlo approach (HMC) for finite temperature simulations. p. 9
Where the paper says it

Our constraint relaxation has been performed using BFGS minimization algorithm by fixing two cell parameters and optimizing the remaining (both length and angle) one. Second-principles The second-principles atomistic simulations were performed using an effective interatomic potential built with the Multibinit package [55], which implements the secondprinciples formalism introduced by Wojdeł et al.

Synchrotron x-ray diffraction measurements were performed at the I16 beamline at Diamond Light Source. p. 9
Where the paper says it

Because the electric field in the CaTiO3 layer lies almost purely in-plane as argued in the previous paragraph, we can calculate its value simply by dividing the voltage by the electrode spacing. Synchrotron x-ray diffraction Synchrotron x-ray diffraction measurements were performed at the I16 beamline at Diamond Light Source [52], using a photon energy of 9.

The analysis of electrical measurements involved simulating the capacitance of an NdGaO3 substrate and subtracting the corresponding charge from experimental data to extract polarization-electric field loops. p. 9
Where the paper says it

Finally, we numerically solve for the dielectric constant of the thin film layer that reproduces the measured capacitance for each temperature or voltage. To extract the polarisation-electric field loops of CaTiO3 thin films from the measured chargevoltage loops, we simulate the capacitance of an NdGaO3 substrate as described in the previous paragraphs and subtract the corresponding charge from the experimental data.

The authors also performed Nudged Elastic Band (NEB) calculations to compute the minimum-energy path connecting polarization states. p. 5
Where the paper says it

3 (a)) and look for the associated switching pathways. We first compute the minimum-energy path connecting the two experimentally accessible polarization states (P21nm ground state and P b21m metastable phase) using secondprinciples nudged elastic band (NEB) calculations (Fig.

The energy versus angle calculation was fitted using Eq. p. 5
Where the paper says it

2(d)), highlighting an abrupt jump associated with a first-order transition. (c) Energy along the same minimum-energy path shown in panel (a), plotted as a function of the rotation angle θ, and its evolution under electric field applied along ⃗bo, as fitted with Eq.

(S1) derived from a minimal angular expansion. p. 6
Where the paper says it

To capture the NEB energy profile U along the minimum-energy path (Fig. 3 (a)) in a compact form, we consider that it only depends on the orientation θ – respect to ⃗ao – of the spontaneous polarization of amplitude Ps, assumed to be constant, and we fit U(θ) using a minimal angular expansion: U(θ) = U0+K1 sin2 θ+K2 sin4 θ+K3 sin6 θ (1) This fit (Table S3) perfectly reproduces both the relative depth of the two minima and the barrier separating them (Fig.

The electrocaloric effect was computed following the method of Ref [64]. The authors also performed atomic force microscopy characterisation of the surface morphology of CaTiO3 films. p. 8
Where the paper says it

Laboratory x-ray diffraction High-resolution x-ray diffraction measurements were performed on a Panalytical X’Pert Pro diffractometer with a Cu-Kα source. Atomic force microscopy AFM topography measurements were performed using tapping mode on a Veeco Multimode IV AFM equipped with a SPECS Nanonis 4 controller using MikroMasch HQ:NSC15/Al BS AFM tips with a force constant of ≈40 N m−1 .

Supplementary Information Details

The supplementary information provides detailed lattice parameters, strain calculations, and atomic force microscopy topography measurements for both (110)o and (001)o orientations. The space group determination confirms that the oxygen octahedral rotations and A-cation antipolar motion persist in the polar phase. p. 1

Where the paper says it

RESULTS We first examine how tensile epitaxial strain can induce and stabilize different polar states in CaTiO3. In bulk, CaTiO3 adopts an orthorhombic P bnm phase which can be seen as a small distortion of the reference cubic perovskite structure: it arises from the condensation of in-phase and anti-phase rotations of the oxygen octahedra according to a pattern (a −a −b +) in Glazer notation [31], and further includes secondary antipolar motions of the Cacations [32] in the plane perpendicular to the in-phase rotation axis of the oxygen octahedra.

Figure S3 shows the energy versus angle θ obtained by fitting Eq. p. 1
Where the paper says it

2 In magnetic systems, double-hysteresis loops in magnetization versus magnetic field (M-H) curves are not restricted to antiferromagnets but can also appear as a feature of some ferromagnetic systems showing first-order magnetization process [18, 19]. In such systems, the free energy shows two slightly inequivalent extrema associated with distinct orientations of the magnetization.

(S1) for CaTiO3 strained on NdGaO3 (110)o and NdGaO3 (001)o. p. 4
Where the paper says it

(b) Experimental dielectric constant versus temperature measurement for the same film as panel (a), along ⃗apc and ⃗bpc, showing a characteristic peak at Tc,exp = 110 K signifying the transition from Pm to P21/m phase. (c) Second-principles polarization versus electric field curve for CaTiO3 strained on NdGaO3 (110)o along ⃗apc and ⃗bpc at Tsim = 40 K in Pm phase.

The results confirm that polarization rotation manifests not as a smooth response, but as a first-order switching process, giving rise to double hysteresis loops. p. 7
Where the paper says it

In contrast, the strain-engineered energy landscape considered here brings competing ferroelectric minima into close energetic proximity, enabling a field-induced polarization reorientation at much lower, experimentally accessible fields. As a result, polarization rotation manifests not as a smooth response, but as a first-order switching process, giving rise to double hysteresis loops.

The predicted electrocaloric temperature change shows opposite signs depending on the field orientation. p. 7
Where the paper says it

Indeed, in magnetic systems, first-order magnetization process is often accompanied by magnetocaloric effects [45, 46] of opposite sign depending of the orientation of the applied field; by analogy, first-order polarization process is expected to couple to similar electrocaloric behaviors. Consistent with this picture, we predict from our second-principles model opposite signs of the electrocaloric temperature change depending on field orientation: ∆T < 0 when the electric field is applied perpendicular to the polarization and is in the same range of efficiency compared to conventional antiferroelectics (∆T /∆E 2 = −3×10-5 K cm2 kV-2) [47, 48].

This duality offers a unique platform combining energy storage, non-volatile memory operation, electrocaloric effects of both signs, and neuromorphic functionalities within a single ferroic system. p. 8
Where the paper says it

A key outcome is that ferroelectric and antiferroelectric-like functionalities coexist within the same material, under identical structural and thermodynamic conditions, and can be selectively accessed by the orientation of the applied electric field. This duality offers a unique platform combining energy storage, non-volatile memory operation, electrocaloric effects of both signs, and neuromorphic functionalities within a single ferroic system.

The authors also provide detailed plots for dielectric susceptibility and change in temperature under different electric field conditions. p. 4
Where the paper says it

Temperaturedependent dielectric measurements in Fig. 2(e) provide an independent manifestation of this duality and anisotropic response, revealing markedly different dielectric signatures depending on the orientation of the applied electric field.

The paper concludes that strain-engineered ferroelastic and antipolar materials are promising candidates for first-order polarization processes. p. 8
Where the paper says it

This duality offers a unique platform combining energy storage, non-volatile memory operation, electrocaloric effects of both signs, and neuromorphic functionalities within a single ferroic system. More broadly, our results establish first-order polarization processes as a general framework for designing multifunctional ferroelectrics, and suggest that strain-engineered ferroelastic and antipolar materials constitute a fertile playground for discovering analogous behavior beyond conventional antiferroelectrics.

Green — the paper says it, and the page is printed. Red — no passage carries it, so treat that sentence as unverified. The same check runs on your own text: check a summary against its source, $5.

Improvements for AI systems

  1. System can predict material response under applied electric fields by identifying if a first-order polarization process is active, which enables double hysteresis P-E loops in ferroelectric materials instead of relying on conventional antiferroelectric ground states.

  2. AI can design novel thin film structures using epitaxial strain to tune the energy landscape of materials like CaTiO3, stabilizing multiple ferroelectric states and engineering the barrier separation between them for controllable switching.

  3. The improved system can classify material behavior into single or double hysteresis loops based on the orientation of the applied electric field, providing a predictive tool for device design in neuromorphic computing and energy storage.

  4. The AI can predict electrocaloric effects with opposite signs depending on field orientation, allowing for the design of multifunctional systems that exhibit both ferroelectric and antiferroelectric-like functionalities simultaneously.

Abstract

Antiferroelectrics generate significant interest since their polarization versus electric field (P-E) curves show typical double-hysteresis loops appealing for various applications. Unfortunately, antiferroelectrics are rare. In magnetic compounds, magnetization versus magnetic field (M-H) curves can show analogous double hysteresis loops not only in antiferromagnets but also in systems exhibiting field-induced first-order reorientation of the magnetization through a so-called first-order magnetization process. Here, we show that appealing double-hysteresis P-E loops can also appear from an unprecedented first-order polarization process. Focusing on non-polar CaTiO3, which can be turned ferroelectric under tensile strain, we study epitaxial thin films on differently-oriented NdGaO3 substrates using a combination of theoretical and experimental techniques. We uncover that a certain configuration exhibits double-hysteresis P-E loops that we rationalize from a field-induced abrupt rotation of the polarization. Such a first-order polarization process establishes a promising alternative pathway to achieve double hysteresis P-E loops appealing for practical applications.